File:A microstructure comparison between the tungsten penetrator of the conventional manufacturing process and the self-sharpening tungsten penetrator manufactured by the cyclic heat-treatment process.jpg
Size of this preview: 800 × 356 pixels. Other resolutions: 320 × 142 pixels | 974 × 433 pixels.
Original file (974 × 433 pixels, file size: 184 KB, MIME type: image/jpeg)
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 02:48, 18 August 2024 | 974 × 433 (184 KB) | Gasiseda | Replaced with the original image with the added white line | |
05:13, 16 August 2024 | 330 × 151 (17 KB) | Herostratus | Add white line separating left and right views, for clarity | ||
19:50, 23 July 2024 | 948 × 433 (221 KB) | Gasiseda | Uploaded a work by 국방과학연구소 - Agency for Defense Development (ADD) from File:ADD's R&D project - Kinetic energy-based 120mm surface penetrator material.jpg with UploadWizard |