File:Alumina nanobottles+setup.jpg

Original file (1,883 × 2,322 pixels, file size: 887 KB, MIME type: image/jpeg)

Description Experimental setup: (a) schematic and (b) photograph. (c) Representative SEM image of the free-standing cluster of alumina nanobottles after etching in phosphoric acid. The scale bar is 500 nm.
Date
Source http://iopscience.iop.org/1468-6996/15/4/045004/article
Author Jinghua Fang et al.
Permission
(Reusing this file)
w:en:Creative Commons
attribution
This file is licensed under the Creative Commons Attribution 3.0 Unported license.
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.

Captions

Add a one-line explanation of what this file represents

Items portrayed in this file

depicts

image/jpeg

3144c8ef4e233d50589ace729e4bbafe76411a13

908,245 byte

2,322 pixel

1,883 pixel

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current04:00, 2 September 2014Thumbnail for version as of 04:00, 2 September 20141,883 × 2,322 (887 KB)Materialscientist{{Information |Description=Experimental setup: (a) schematic and (b) photograph. (c) Representative SEM image of the free-standing cluster of alumina nanobottles after etching in phosphoric acid. The scale bar is 500 nm. |Source=http://iopscience.iop.o...

The following page uses this file: