File:Change of hardness with aging.tif

Original file (628 × 609 pixels, file size: 1.09 MB, MIME type: image/tiff)

Summary

Description
English: Change of hardness (measured using diamond Vicker indent and expressed in Vickers Pyramid Number, HV) with 2, 4, 8, 16, 32, 64, and 128 hours aging time for the ferrite phase in super-duplex Zeron 100 alloy
Date
Source In situ full-field characterisation of strain concentrations (deformation twins, slip bands and cracks)
Author A. Koko

Licensing

I, the copyright holder of this work, hereby publish it under the following license:
w:en:Creative Commons
attribution share alike
This file is licensed under the Creative Commons Attribution-Share Alike 4.0 International license.
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
  • share alike – If you remix, transform, or build upon the material, you must distribute your contributions under the same or compatible license as the original.

Captions

Add a one-line explanation of what this file represents

Items portrayed in this file

depicts

2 March 2023

image/tiff

3e98cc9fad003659cd9ed441c9b3da6810ce5ff6

1,148,139 byte

609 pixel

628 pixel

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current10:32, 2 March 2023Thumbnail for version as of 10:32, 2 March 2023628 × 609 (1.09 MB)FuzzyMagmaUploaded own work with UploadWizard

The following page uses this file:

Metadata